The influence of 2.0% nickel on thin and section permanent molded austempered ductile iron samples were investigated for abrasion and erosion behavior. The section sizes of samples were varied at two levels viz. 25 mm and 50 mm. Wind turbine hubs which were subjected to wear and erosion were made from thin and thick section PMADI castings. The austempering temperature and time were optimized for improved wear behavior and strength at 3000 C for 60 mins. Nickel additions showed about 7% improvement in the wear resistance of thin section PMADI samples over unalloyed PMADI samples. For the purpose of comparison, sand-cast austempered ductile iron was also evaluated for abrasion, erosion resistance. Thin section (25 mm) PMADI samples subjected to austempering at 3000 C for 60 mins showed improved abrasion and erosion behavior in addition to higher strength values over thick section (50 mm) PMADI and sand cast ADI samples. Further these data were analyzed with structure property correlation and were well supported by light photomicrographs.

Keywords

PMADI, Thin/thick section, Abrasion\erosion and Wind turbine hubs
User
Subscription Login to verify subscription
Notifications
Font Size

Abstract Views: 241

PDF Views: 0




  • Influence of Nickel on Abrasion and Erosion Wear Behavior of Thin and Thick Section Permanent Molded Austempered Ductile Iron for Wind Turbine Hubs

Abstract Views: 241  |  PDF Views: 0

Authors

K. Narasimha Murthy
Department of Mechanical Engineering, CMR Instituteof Technology, Bangalore, India
P. Sampathkumaran
Central Power Research Institute, Bangalore - 560 010, India
Seetharamu S.
Central Power Research Institute, Bangalore - 560 010, India
R. K. Kumar
Central Power Research Institute, Bangalore - 560 010, India

Abstract


The influence of 2.0% nickel on thin and section permanent molded austempered ductile iron samples were investigated for abrasion and erosion behavior. The section sizes of samples were varied at two levels viz. 25 mm and 50 mm. Wind turbine hubs which were subjected to wear and erosion were made from thin and thick section PMADI castings. The austempering temperature and time were optimized for improved wear behavior and strength at 3000 C for 60 mins. Nickel additions showed about 7% improvement in the wear resistance of thin section PMADI samples over unalloyed PMADI samples. For the purpose of comparison, sand-cast austempered ductile iron was also evaluated for abrasion, erosion resistance. Thin section (25 mm) PMADI samples subjected to austempering at 3000 C for 60 mins showed improved abrasion and erosion behavior in addition to higher strength values over thick section (50 mm) PMADI and sand cast ADI samples. Further these data were analyzed with structure property correlation and were well supported by light photomicrographs.

Keywords


PMADI, Thin/thick section, Abrasion\erosion and Wind turbine hubs



DOI: https://doi.org/10.33686/prj.v9i2.189582