Transvarestraint Testing of Low Ferrite Consumables for Austenitic Stainless Steel Welding


Affiliations
1 Metallurgical Engineering Department, M, S. University of Baroda, Vadodara, India
     

   Subscribe/Renew Journal


Two low ferrite filler wires and one autogenous weld were tried on 316L Stainless Steel sample plates, lor assessing the hot cracking susceptibility. The deposited welds were tested for ferrite number and the autogenously melted using TIG process on Transvarestraint testing unit. These samples were strained at two different levels. The hot cracking susceptibility was measured in terms of number of cracks, total length of cracks and maximum crack length at two different strains to the weld metal. It was found that the total crack length or number of cracks are indicative of cracking susceptibility. Interestingly, order of increasing susceptibility in the welded samples matched with the decreasing level of delta ferrite.
User
Subscription Login to verify subscription
Notifications
Font Size

Abstract Views: 294

PDF Views: 5




  • Transvarestraint Testing of Low Ferrite Consumables for Austenitic Stainless Steel Welding

Abstract Views: 294  |  PDF Views: 5

Authors

S. K. Agrawal
Metallurgical Engineering Department, M, S. University of Baroda, Vadodara, India
M. N. Patel
Metallurgical Engineering Department, M, S. University of Baroda, Vadodara, India

Abstract


Two low ferrite filler wires and one autogenous weld were tried on 316L Stainless Steel sample plates, lor assessing the hot cracking susceptibility. The deposited welds were tested for ferrite number and the autogenously melted using TIG process on Transvarestraint testing unit. These samples were strained at two different levels. The hot cracking susceptibility was measured in terms of number of cracks, total length of cracks and maximum crack length at two different strains to the weld metal. It was found that the total crack length or number of cracks are indicative of cracking susceptibility. Interestingly, order of increasing susceptibility in the welded samples matched with the decreasing level of delta ferrite.